Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to find the amount of precambering to be done before welding to avoid distortion?

krish2002

Mechanical
May 5, 2025
1
How to find the amount of precambering to be done before welding to avoid distortion?
 
Replies continue below

Recommended for you

A sketch would be helpful, to broad of a question.
It depends case by case, and what is your definition of precambering?
 
trial and error ?

I doubt that the warping of a weldment is calculatable (is that a word ? look odd).

I'd suggest heat treatment to relieve the stresses due to welding.
 
Practice is the way.

We had a supplier come back on a re-procurement contract and "explain" how the part could not be made as they had repeatedly failed to make a suitable weldment.

Their welder was trained in the Air Force for structural repairs; all his welds were defect free. They also were huge. Ginormous. Fat. Since nearly 100 had previously been made by a different supplier, we know it was possible - eventually the original welder was willing to go and show their guy how to put down a suitable bead, fast, defect free. The fat welds? 2-3 days per unit. The desired welds - 2-3 units get welded in a day.

Tackling deformation due to welding is a tough thing - it depends on how the part is restrained, how much the surrounding metal is heated, how much the melt zone shrinks with the dropping temperature which depends on how big the melt zone is. It very much depends on if the welding is symmetric or not, it depends on how fast the welder goes (affecting the size of the melt zone and the surround material expansion). Sometimes it depends on the crystalline state of the various components, going from face-centered cubic to body-centered cubic in the case of carbon steel.

Set up trial pieces and see how much deformation occurs with different approaches and how uniform the results are from some single approach.
 