I have to conduct a Lab tests (Corrosion) tests on a material ( The objective is to evaluate the weight loss/Rate of corrosion in service). Service fluid is known and pressures are known and the operating temperatures are known.

Life of the item is designed for 20 years.

I need an ASTM/BS/EN/ISO general test guidance note or international acceptance practice that specify the accelerated test duration and test temperature, so that the test results can reasonably be co related/extrapolated to service life.

Thanks in advance.
 
Good Luck!

I ususally put very little faith in accelerated lab tests for prediction of actual service life. For example, 1000 hours in a salt-fog chamber relates to......1000 hours in a salt fog chamber!

Before saying anything more in that light, can you provide a little more info?

- what is the service environment; what is the proposed accelerated test(s); etc.
 
First you need to do some short term lab testing and look at your corrosion mechanism. Run tests at different durations and compare the results.
IF you are dealing with uniform corrosion.
And IF you can show that there are no 'breakaway' conditions.
Then maybe you can figure out how to raise the temp and pressure some to accelerate the testing.

Or can you find a standard test that creates the same type of corrosion? Then you could use that method.

= = = = = = = = = = = = = = = = = = = =
Corrosion, every where, all the time.
Manage it or it will manage you.
 
Whoever specified the tests in the first place should have thought about all of that. There's whole libraries on the subject and you want it solved on a forum like this? Go back to the people who requested the test and ask them exactly what are they looking for and how they want it obtained.

Steve Jones
Materials & Corrosion Engineer
 
Thn you SJones for your VERY VALUABLE POST !! (AS USUAL as attacking as Corrosion of CS in Sea Water)
 