I want to make purchasing ordre , but how to make choise material for well head equipements.


Thanks
 
Get the Materials & Corrosion Engineer to document the materials in a materials selection report.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
API 6A has recommendation in regard with production specific level PSL.
NACE MR 0175 has specs for sour service and other materials used in corrosive environments. Based on calculated partial pressure some companies might have other (usually more stringent)requirements on material used.
Provincial and government regulations have to be taken in account as well. In AB, a critical sour well has to have a PSL3 WH, even-though API 6A recommends a PSL2 WH.

If you speak with WH manufacturer they will know this stuff and head you in the right direction.
 
The WH manufacturer will try to sell whatever is most commercially convenient. It is down to the end user to be very specific about what is required.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 