I am making a large diameter (~23" OD, ~21.5 ID ) tube with a 20mm thick H8PP NidaCore core.
The tube will be used for a large telescope and needs to be stiff but it will not by carrying any significant weight as the entire telescope will only weigh about 85 lbs.
How many plys of 11 oz 8HS carbon cloth should I use for the inner and outer layers? I would think that 1 ply (with perhaps a 12" overlap at the seam) would be sufficient and result in a very stiff tube.
I have made one other tube about this size and used two plys of 11 oz cloth for each layer. The tube had a .250" Flexcore core and was super stiff. I tried to flex the tube by giving it a bear hug and I couldn't get it to budge in the slightest. I'd like to save money where possible yet not compromise strength, hence, my question about going with 1 ply for each layer versus 2.
I will be vacuum bagging the tube in probably three layup steps (inner, core, outer) using peel ply to get a good bondable surface between the inner layer and the core.
Thanks,
Dave
The tube will be used for a large telescope and needs to be stiff but it will not by carrying any significant weight as the entire telescope will only weigh about 85 lbs.
How many plys of 11 oz 8HS carbon cloth should I use for the inner and outer layers? I would think that 1 ply (with perhaps a 12" overlap at the seam) would be sufficient and result in a very stiff tube.
I have made one other tube about this size and used two plys of 11 oz cloth for each layer. The tube had a .250" Flexcore core and was super stiff. I tried to flex the tube by giving it a bear hug and I couldn't get it to budge in the slightest. I'd like to save money where possible yet not compromise strength, hence, my question about going with 1 ply for each layer versus 2.
I will be vacuum bagging the tube in probably three layup steps (inner, core, outer) using peel ply to get a good bondable surface between the inner layer and the core.
Thanks,
Dave