We are planning to perform a double hot-tap and stopple on 10" pipe SCH STD with AGO as a process fluid from a distillation tower. The pressure for the process is 54 psi and the temperature is 440°F. The hot-tap company asked us for a maximun velocity through the pipe of 4 feet/sec. We have an internal document called Guidelines for Hot-tap and it is recommended a velocity not greater than 6 ft/sec. Can anybody tell me why we should control the process fluid velocity and what could be the consequences of not doing that?

Best regards,
M.D
 
Replies continue below

Recommended for you

In very general terms: With little or no fluid movement you get more decomposition of the fluid; With high fluid velocities you carry weld heat away faster giving more quench = hardness +low toughness. The latter is less of a concern with your 440F, it is more relavent to ambient temp flow lines. My guess is that the Guidlines were written for ambient temp work.
 