Is it prohibited by ASME Section VIII Div1 that a repad be formed at a temperature 300 to 400°C ?
This repad SA516Gr70 will reinforce an opening at the knuckle of the head of a pressure vessel. The complete PV will be subjected to PWHT per UCS-56
 
Replies continue below

Recommended for you

It is not prohibited. Since you are performing PWHT fiber elongation is not a problem.
 