Hello everyone.
Our project requires subbase courses to be compacted to not less than 100% standard compaction. The contractor's compaction report submits a test report as Hilf density ratio being 102%. Can this be intepreted as compliant having exceeded the requirement by 2%? So for subgrade compaction requirement of 97%, the same interpretation applies.
Thanks for replying.
Our project requires subbase courses to be compacted to not less than 100% standard compaction. The contractor's compaction report submits a test report as Hilf density ratio being 102%. Can this be intepreted as compliant having exceeded the requirement by 2%? So for subgrade compaction requirement of 97%, the same interpretation applies.
Thanks for replying.