Can someone please guide me that which stainless steel material grade is suitable for the below operating condition?

Continuous Operating temperature is:1000 DegC in a sulfurous environment

 
I recommend paying attention to 316L stainless steel. it is often used for such environments and is able to withstand the required temperature.