I need to run a solenoid at 500 deg C around 300 V for R&D work.
6-10 amps
No cooling available.
Continuous duty

Apart from resistance effects of temperature most insulations will be breaking down at temperatures above 150 deg. C

Coil must be fairly compact and wound like traditional solenoid so thick insulation like ceramic beads not feasible.

Can anybody recommend anything?

Many thanks.
 
Replies continue below

Recommended for you

Use air for insulation.
Cut the conductor from the solid, like a Heli-Cal coupling.



Mike Halloran
Pembroke Pines, FL, USA
 
You can consider copper tubes wound helically, and cooled internally with water circulation. Electrical insulation,you could have as per your desire.

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Can you wind a free-standing coil and then repeatedly dip in a slurry, similar to what they do for investment casting? I believe that is what the do for some power resistors.
 
Look at anodized aluminum strip.

Mike
 