Hercules28
Materials
- Nov 9, 2010
- 169
Hi all,
I am looking for a high strength dielectric washer (>100ksi yield)
I have a test setup of Inconel to Steel in a Salt Spray chamber.
I am aware of the potential for galvanic action and I am looking for a high strength dielectric. The force between Inconel and Steel will be max ~100ksi
Any Ideas?
I also read in the forum about LanoCote and Tef Gel as coatings.
this is a 10 day test so it doesn't have to last forever.
The Inconel is required for strength and to also not corrode in the salt spray.
I can consider alternatives to the Inconel..however they need to be very strong and not corrode.
What I am testing is the Steel under stress. Inconel is used to create stress.
Thanks,
Herc
I am looking for a high strength dielectric washer (>100ksi yield)
I have a test setup of Inconel to Steel in a Salt Spray chamber.
I am aware of the potential for galvanic action and I am looking for a high strength dielectric. The force between Inconel and Steel will be max ~100ksi
Any Ideas?
I also read in the forum about LanoCote and Tef Gel as coatings.
this is a 10 day test so it doesn't have to last forever.
The Inconel is required for strength and to also not corrode in the salt spray.
I can consider alternatives to the Inconel..however they need to be very strong and not corrode.
What I am testing is the Steel under stress. Inconel is used to create stress.
Thanks,
Herc