I have an application where I need to bond two small 7075 Aluminum housings together (permanently); the bonded assembly must withstand ~2500 psi and ~300 degrees F with no pressure bleed-though into the small interior cavity.

Any suggestions on how best to accomplish this?

Thanks,

Mike
 
Replies continue below

Recommended for you

Have you considered buring "o" rings" (c/w grooves) in the sealing system?
 
I have considered o-rings, but implementation would be difficult at best due to outside envelope and interior volume requirements. Another option I am currently exploring is a material change to 6061 and a post assembly welding operation (laser or EB).

-Mike
 