TPU is a high performance polyester/polyether based thermoplastic polyurethane elastomer for extrusion.
I need to know the porosity of the material or how likely is it to absorb moisture??

FYI
Some other properties:
Grade Resilience: JSI-S8500
Hardness: Shore A85
Tensile Strength: 350 kgs/sq cm
Elongation: 600%
Impact: 40%
 
Replies continue below

Recommended for you

Cant help you on this question but BASF in germany make elastollan and they will have the answer
regards from sout africa
fred evans
polyflexseals
 