Thanks.
The steel in question is part of a burner lance in a cement kiln...1500 deg C. The lance is encased in a refractery, but I was curious what effects temperature has on the steel alone. I suppose it is not a valid question, the refractery must be there or the steel will melt.
Forgeting the high temperature of the kiln, is there a rule of what happens to yield stress and modulus at high temeratures?