Gas exiting amine plant is increasing the pH of TEG solution within the dehydration plant downstream.
pH has gone as high as pH 10. we seek information from those with experience. How can we bring down the pH to acceptable level.
What is the acceptable level and what chemical can we use, and at what point is best to inject the chemical.
Literature sources suggest phospkoric or acetic acid.
Kindly assist
regards
productqualitycontrol
pH has gone as high as pH 10. we seek information from those with experience. How can we bring down the pH to acceptable level.
What is the acceptable level and what chemical can we use, and at what point is best to inject the chemical.
Literature sources suggest phospkoric or acetic acid.
Kindly assist
regards
productqualitycontrol