Hi;
I am having bearings high temperature problems. The machines are GE electrical motor Model 5KS447SS146D8, Horsepower 200 HP, Frame 447TS, 3 Phases, 3570 RPM, 460 Volt, 60 Hertz, Enclosure TEFC, Insulation Class F, Bearing DE/ODE 6314ZC3, driven two Sulzer 9 stage centrifugal pump size 3x4x8.75A MSE
These motors seems to run since star up (about 6 years ago) with high DE bearing temperature over 200°F and max. 208°F (measured with a infrared thermometer), causing premature bearing failure, we lubricate with Mobilith SHC 100. Running the motor with no load the maximum temperature found was 136°F after 2 hours running.
We have done several test and we have found nothing abnormal.
1.Check current and voltage with no load and load.
2.Check alignment motor-pump, inspect coupling condition, coupling hub distance, motor shaft runout, even tough there were no high vibration condition.
3.Replace bearings, check over/lack lubrication condition, check bearing outer race/motor bearing housing clearances and bearing inner race/shaft clearances.
Could you please tell me if I am missing something?
Regards.
I am having bearings high temperature problems. The machines are GE electrical motor Model 5KS447SS146D8, Horsepower 200 HP, Frame 447TS, 3 Phases, 3570 RPM, 460 Volt, 60 Hertz, Enclosure TEFC, Insulation Class F, Bearing DE/ODE 6314ZC3, driven two Sulzer 9 stage centrifugal pump size 3x4x8.75A MSE
These motors seems to run since star up (about 6 years ago) with high DE bearing temperature over 200°F and max. 208°F (measured with a infrared thermometer), causing premature bearing failure, we lubricate with Mobilith SHC 100. Running the motor with no load the maximum temperature found was 136°F after 2 hours running.
We have done several test and we have found nothing abnormal.
1.Check current and voltage with no load and load.
2.Check alignment motor-pump, inspect coupling condition, coupling hub distance, motor shaft runout, even tough there were no high vibration condition.
3.Replace bearings, check over/lack lubrication condition, check bearing outer race/motor bearing housing clearances and bearing inner race/shaft clearances.
Could you please tell me if I am missing something?
Regards.