Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

HELP

Status
Not open for further replies.

Peter

New member
Feb 1, 1999
16
Does anyone have experience with producing Class A finishes with the SCRIMP process using vinylester resin and core materials. We are a boat builder, and have a solution, but we are looking for alternate ways around the problem
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor