I have to choose materials for the following equipment with parameters as under:
Separator
medium = oil, gass, water * pressure 16 bar * temp 67 deg C * Partial pressure CO2=0,06 bar * 280ppm H2S
Gas Cooler
medium = oil, gass, water,seawater * pressure 3 bar * temp 37 deg C * Partial pressure CO2=0 bar * 280ppm H2S
Cooler
medium = oil, gass, water * pressure 36 bar * temp 50 deg C * Partial pressure CO2 0,04 bar * 280ppm H2S
Cooler
medium = oil, gass, water * pressure 139 bar * temp 73 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
Scrubber
medium = oil, gass, water * pressure 11 bar * temp 30 deg C * Partial pressure CO2 0,04 bar * 280ppm H2S
Scrubber
medium = oil, gass, water * pressure 138 bar * temp 88 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
Compressor
medium = oil, gass, water * pressure 138 bar * temp 88 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
need materials with low density because of weight problems.
Can anyone help me??
Separator
medium = oil, gass, water * pressure 16 bar * temp 67 deg C * Partial pressure CO2=0,06 bar * 280ppm H2S
Gas Cooler
medium = oil, gass, water,seawater * pressure 3 bar * temp 37 deg C * Partial pressure CO2=0 bar * 280ppm H2S
Cooler
medium = oil, gass, water * pressure 36 bar * temp 50 deg C * Partial pressure CO2 0,04 bar * 280ppm H2S
Cooler
medium = oil, gass, water * pressure 139 bar * temp 73 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
Scrubber
medium = oil, gass, water * pressure 11 bar * temp 30 deg C * Partial pressure CO2 0,04 bar * 280ppm H2S
Scrubber
medium = oil, gass, water * pressure 138 bar * temp 88 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
Compressor
medium = oil, gass, water * pressure 138 bar * temp 88 deg C * Partial pressure CO2 0,57 bar * 280ppm H2S
need materials with low density because of weight problems.
Can anyone help me??