Dec 13, 2009 #1 keluonuosi Mechanical Joined Jul 12, 2009 Messages 10 Location CN anyone can tell me what's the Threadlock eslock.And if can tell me its detail,its more good. Thanks!
Dec 13, 2009 1 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Eslock is a polyamide thread patch. More information here: http://www.anochrome-group.co.uk/plastic_patch.asp In general, these offer limited performance advantage. If you need sealing and/or vibration resistance, then thread adhesives would be a better choice. Upvote 0 Downvote
Eslock is a polyamide thread patch. More information here: http://www.anochrome-group.co.uk/plastic_patch.asp In general, these offer limited performance advantage. If you need sealing and/or vibration resistance, then thread adhesives would be a better choice.
Dec 14, 2009 1 Thread starter #3 keluonuosi Mechanical Joined Jul 12, 2009 Messages 10 Location CN oh, eslock is eslok. I got this.Thanks. Upvote 0 Downvote