Team
I'm a rubber eng, but i have to do an analysis on a plastic cracking/breaking
The FTIR concludes the presence of an Oil similar to Castor Oil or Tall Oil.
There is a plastic casing an a wire wrapped comming inside of the casing.
Any idea or where does it can came, Wire wrap, plastic case....
I'm a rubber eng, but i have to do an analysis on a plastic cracking/breaking
The FTIR concludes the presence of an Oil similar to Castor Oil or Tall Oil.
There is a plastic casing an a wire wrapped comming inside of the casing.
Any idea or where does it can came, Wire wrap, plastic case....