Hello Engineers
I'm trying to find Material Grade X22CrMoV12-1 (1.4923)
equivalent to in ASTM (UNS No. ) standard please help out if any information available related to it.

Thank you😊🙏

 
You will find your answer if you just Googled it. I would otherwise suggest getting a copy of the ASM reference "Worldwide Guide to Equivalent Iron and Steel Alloys".
 
ASTM A335 P22 Pipe
Trade Name: 2 ¼ Chrome
Grade: P22
UNS #: K21590
Pipe: A335/SA335
Forged/Bored Pipe: A369/SA369


DHURJATI SEN
Kolkata, India


 
Thank you Mr failure, Appreciated I will refer "SAE HS-1086/2017 ASTM DS56L" also I will go through "ASM" too.I marked your post with star.

Hello Dhurjati,
UNS K21590 is 10CrMo9-10 (1.7380)

Finally answer for information is
Material Grade X22CrMoV12-1 (1.4923) is UNS S42200 (SS422).

Thank you 😊 all of you

 