wumbo6
Aerospace
- Apr 24, 2018
- 1
I have a bonded part that I subject to helium vacuum bombing/pressurization and perform leak detection using a mass spectrometer using the helium as a tracer gas. The adhesive I'm using is absorbing the helium during the bombing cycle and releasing it during the detection cycle creating a virtual leak. Can anybody recommend an adhesive or coating that would prevent helium absorption?