I would like to harden 416 stailess steel, what would be the right process and temperatures for this
 
You need to figure out what are your loads and stresses that the part is going to see and then decide what heat treat is necessary.
Edson Campos
edsoncampos@earthlink.net

 
Refer to the ASM Metals Handbook volume 2 for suggested temperatures. You still need to determine the properties required before commencing.

Good Luck
 
losochos: There are many variables in heat-treating, so it's hard to be specific because you have not provided any details (part geometry, type of furnace, etc.). But generally speaking, 416SS is austenitized at 1700-1850 deg F, oil-quenched, then tempered at 1050-1125 deg F. If you use an atmospheric furnace be SURE to double wrap the part or you won't like the result.
 