New process exploration, I imagine I will need a little more detail as well to solve. Where do I start?
CONDITION: With a continuously moving extrusion 30 ft/min going through a die block at 400 deg(f) and using high velocity (100 mi/hr)nitrogen gas -140 deg(f) released inside extrusion for rapid cooling.
QUESTION: What will the resultant temperature balance be in the die, will the nitrogen pull down the die temp or will it be negated as the extrusion is constantly being drawn away.
CONDITION: With a continuously moving extrusion 30 ft/min going through a die block at 400 deg(f) and using high velocity (100 mi/hr)nitrogen gas -140 deg(f) released inside extrusion for rapid cooling.
QUESTION: What will the resultant temperature balance be in the die, will the nitrogen pull down the die temp or will it be negated as the extrusion is constantly being drawn away.