Hello everyone,

Well this time I have to find some 8-10" butterfly and check valves, made from HDPE.
Now, I saw that PVC is the most common type of material and the cheapest as well, I want to know if my requirement of HDPE valves could be replaced by PVC valves?
What would be the advantages or disadvantages of selecting a PVC valves instead of a HDPE valve? My piping will be made from HDPE, so the contraction and expansion of materials would be different, so that is a disadvantage. A water pump will carry water through the piping.

I'm open to your advice.
Thanks very much.
 
Both HDPE and PVC pipes should be fine for water service however HDPE and PVC both have limited resistance against sunlight/UV exposure so trust you already have a shed or some sort of protection.

U-PVC would be the preferred option if the water is supposed to be used for living beings else C-PVC is better for a little higher temperatures.

The other option is to use metallic valves (SS316 for potable water or Ductile iron with coating for other uses).

 