Please I have a question. How can I use hashin damage model for a solid element and not shell? I trued to use for a shell elements and it worked, however, when I tried it for a slid element, it did not. Kinly help me with the step-by-step approach to achieve that.

Thank you for always!
 
Replies continue below

Recommended for you

From the documentation:

The Hashin damage model must be used with elements with a plane stress formulation, which include plane stress, shell, continuum shell, and membrane elements.
 