Dear Experts,

Please advise on below query.

Applicable codes are;
ASME Section IX
NACE MR 0175.

We have one WPS Qualified in butt joint and Hardness survey done according to NACE MR 0175 (7.3.3.3 Figure 2) on Butt weld coupon.

​Is it correct that we cannot use the above WPS in a fillet joint because the fillet weld harness survey is not carried out.