Hi sir ,
i want to ask that how to controlled ferrite % in hardening and quench tempered steel.
after hard and tempered structure observed tempered martensite with 25% ferrite plz tell how to control ferrite level
 
that means if we done with 400-450°C than not much more effect in structure and structure not fully tempered martensite.only stress relief in this temperature for better structure should i go above 500°C tempered.and material is 35C8 grade
 
What strength/hardness do you need? If it is 241-295 HBW, then 500 °C to 550 °C should work.
 
sir hardness required 180-220 BHN after tempering and observed after hardening max 255BHN
 
Why are you quench hardening to achieve 180 HBW? Other options seems better (as rolled, normalized).
 
hi sir,

please suggest to me for reduce decarburization.
actually new development item i have hard n tempered.
but in final micro observed fully decarb.
its socket Wt. 800gm Spec hardness 201-255 BHN
 