Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Hard Particle Bearing Damage

Status
Not open for further replies.

enirwin

Mechanical
Feb 14, 2002
46
I'm looking at a case hardened pump shaft that also serves as an inner race for a needle bearing. The shaft has hard particle dents all over it and is starting to spall in one spot.

How hard does a particle have to be to dent the surface of a steel shaft with a case hardness of HRC60? I have a potential source of cast iron debris at HRC20-30. Would this be hard enough to cause dents?

Any help would be appreciated.

Thanks.
 
Replies continue below

Recommended for you

Yes - even though the case is hard if it is thin and the underlying base material is soft then indendation damage can occur quite easily even with relatively soft particles.
 