Hi,
I've recently sent MPPO & PAS (both glass filled) for lab test to determine the level of flourine & chlorine. To my surprise the level of both elements were very high.

MPPO - flourine : >2000 ppm, chlorine : nd
PAS - flourine : nd, chlorine : >2000 ppm

Upon checking with the material supplier, I later found that the use of PTFE in MPPO is the root cause for high flourine ppm. But unfortunately until this day we still unable to establish the source of chlorine in PAS. The material supplier claim that no chlorine is used througout their process. Could anyone share their thoughts or experience?

Thanks
 
Replies continue below

Recommended for you

Maybe a colour or more likely a flame retardant. Also just possibly a coating on the glass fibre to aid in bonding glass to fibre.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor