I'm working on a material selection study where I have to study a water with a content of 500ppm of H2S dissolved. Since I'm working with ECE software (De Waard and Milliams Model) that use the ppm dissolved in the gas phase. Is it possible to find a correlation beetween the H2S dissolved in the water and the one dissolved in the gas phase considering that the Gas is at 80 barg?
Thanks
 
H2S dissolves in water by dissociation into H+ and HS- at least. Solubility therefore depends on pH (i.e. initial pH and buffering capacity), not just on partial pressure of H2S in the gas.
 