13
I am having a problem with mechanical properties of GX8CrMoAlSi18.3 alloy which contains 0.09% C, 1.00% Si, 0.80% Mn, 18% Cr, 3% Mo, 1% Al. I need to get tensile strength Values above 500 N/mm2, but i only got 320 max. Any comments about the heat treatment will be pleased. Thank you...
 