Hi guys. Any of you have a rough guideline for the number of weld passes vs. pipe size for stick process in CS pipe? For example, for 2" sch 40, I know there is a root pass, hot pass, and cap. AS the size goes up you have to start adding filler passes. If you have the info for XS and XXS that would be great too. GTAW/GMAW need not apply. Ha Thanks guys!