A newly installed 20,000 gallons vertical tank on a two foot thick reinforced concrete slab. Concrete slab is square and roughly 25'X 25'.Two perpendicular grooves,(about 2"X2")running from opposite edges and thru the center the concrete slab were incorporated. I have never seen such large grooves in CB's before. Are these grooves for "telltale" about potential tank bottom leak or are these for crack control?
 
Replies continue below

Recommended for you

FYI - "IF" this foundation had a high point in the center, when a leak did occur you could pin-point the leak origin to a quadrant in the tank.
 
At least pinpoint which half of the bottom is leaking but not whereabout.
 