Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

grit blast process

Status
Not open for further replies.

UchidaDS

Mechanical
Sep 28, 2011
116
I am looking for a type of material that can handle the abrasion of grit blast process. It is basically to serve for masking purpose. I am thinking of using tool steel, perhaps D2 tool steel? Does anybody have any experience on this?
 
Replies continue below

Recommended for you

Try googling tombstone tape.
B.E.

The good engineer does not need to memorize every formula; he just needs to know where he can find them when he needs them. Old professor
 
UchidaDS,

Rubber works well for shot/grit blast masking. It is cheap, durable, and easy to custom mold into tight fitting plugs/sleeves/masks.

Terry
 
Urethane rubber, to be a bit more specific than tbuelna, is easy to hand-pour/cast from two-part mixed solutions, and has very good abrasion resistance.
 
Thanks for all these replies.
I use urethane before, no doubt about it.
For this application, the area to be grit blast is so narrow ( meaning you have obstacle from the source, you have to shot the grit in an angle) and required not to over/under blast the surface. It has only about .25" to be blasted and it is in cylindrical shape.
I don't think that using rubber material I could able to obtain a good seal/strenght to prevent over blast.
 