Grinding on P91 weld joint

Status
Not open for further replies.

tamal1475

Materials
Mar 29, 2012
41
Is there any special precaution to be followed if we grind off surface irregularities on weld joints of heavy walled P91 header pipes? Will it affect if we do the grinding before or after PWHT? The surface ripples on the SMAW weld runs are interfering with the NDT.
 
Replies continue below

Recommended for you

If typical grinding measures are followed as with other weld joints, no.
 
Just remember if MT or PT is required do it after grinding and not before.
 