I am looking for an electrically conductive altenative plating for olive drab cadmium plating. Any suggestions?
 
Replies continue below

Recommended for you

Depending on how much your you need eletroless nickel is good bet.
If it is a simle shape use could use chrome or nickel electroplate as it seem to be since you are cadmium plating now.

If you could give a little more information someone can get a little more detailed.
 