Hello,
I am procuring gasket sheet for different equipment's used in refinery. The specifications are as follows:
Size: 2m X 1.5M X 3mm Thick
Material: Graphite sheet reinforced with SS316 Wire mesh
Specification; As per ASTM F36 A
MAX Working Pressure: 200bar
MAX working Tepmrature: 500 Centigrade
Type: Soft Cut
Some suppliers are quoting for gasket sheet reinforced with Tanged insert Stainless steel instead of wire mesh reinforcement. How may I confirm from any applicable code that which type of reinforcement is better or both type of reinforcement is acceptable under different pressure and temperature conditions. Please identify the difference of both based on their pressure bearing capacity and which is more better among the two options.
Best Regards,
I am procuring gasket sheet for different equipment's used in refinery. The specifications are as follows:
Size: 2m X 1.5M X 3mm Thick
Material: Graphite sheet reinforced with SS316 Wire mesh
Specification; As per ASTM F36 A
MAX Working Pressure: 200bar
MAX working Tepmrature: 500 Centigrade
Type: Soft Cut
Some suppliers are quoting for gasket sheet reinforced with Tanged insert Stainless steel instead of wire mesh reinforcement. How may I confirm from any applicable code that which type of reinforcement is better or both type of reinforcement is acceptable under different pressure and temperature conditions. Please identify the difference of both based on their pressure bearing capacity and which is more better among the two options.
Best Regards,