APPLICATION: Heavy duty trucks make use of king pins and bushings as part of their steering pivot points. The king pins are held in place with tapered threaded draw keys. Basically, the king pins have notches on their sides that allow a tapered draw key to be inserted and pounded in place. Then the draw key is secured in place with a locknut.
DESCRIPTION: Currently, we fabricate all of our own draw key hardware for the king pin kits we produce.
We purchase AISI 4140 rod material, fabricate it and heat treat it (surface hardness to 28 HRC to 34 HRC) to print specifications.
To date, not one complaint has ever arisen regarding draw key hardware failure.
That being said, our largest customer has recently specified that we must, among other things, place a grade on all of our hardware we produce for them to continue purchasing our products.
Now I am familiar with hardware grade markings and various hardware grade charts. However, I am very unfamiliar with the methods/specifications/standards used by hardware manufactures to establish a grade on hardware.
QUESTION: What method is used by hardware manufacturers to rate/specify bolt grades? Are standards available?
Thanks.
Regards,
Tim Kaiser
VW Kaiser Engineering, Inc.
DESCRIPTION: Currently, we fabricate all of our own draw key hardware for the king pin kits we produce.
We purchase AISI 4140 rod material, fabricate it and heat treat it (surface hardness to 28 HRC to 34 HRC) to print specifications.
To date, not one complaint has ever arisen regarding draw key hardware failure.
That being said, our largest customer has recently specified that we must, among other things, place a grade on all of our hardware we produce for them to continue purchasing our products.
Now I am familiar with hardware grade markings and various hardware grade charts. However, I am very unfamiliar with the methods/specifications/standards used by hardware manufactures to establish a grade on hardware.
QUESTION: What method is used by hardware manufacturers to rate/specify bolt grades? Are standards available?
Thanks.
Regards,
Tim Kaiser
VW Kaiser Engineering, Inc.