Feb 25, 2020 #1 GAL02 Mechanical Joined Sep 2, 2015 Messages 55 Location KW Good afternoon to all! I came across term 'SRWN' RF flange during PV Dwg.overlook. As I know LWN flange as 'Long weld neck flange' but what is 'SRWN' flange? Is it Short Radius Weld Neck (SRWN)Flange? Pl. revert. With regards
Good afternoon to all! I came across term 'SRWN' RF flange during PV Dwg.overlook. As I know LWN flange as 'Long weld neck flange' but what is 'SRWN' flange? Is it Short Radius Weld Neck (SRWN)Flange? Pl. revert. With regards
Feb 25, 2020 #2 HTURKAK Structural Joined Jul 22, 2017 Messages 3,371 thread794-205538 Upvote 0 Downvote
Feb 26, 2020 Thread starter #3 GAL02 Mechanical Joined Sep 2, 2015 Messages 55 Location KW Hi! It's just Merry-go-round! With regards Upvote 0 Downvote
Mar 1, 2020 #4 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN Dear GAL02, Could be a short radius elbow attached to a weld neck flange. I would visit the site to actually locate the subject and clear all doubts. Regards. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Dear GAL02, Could be a short radius elbow attached to a weld neck flange. I would visit the site to actually locate the subject and clear all doubts. Regards. DHURJATI SEN Kolkata, India
Mar 1, 2020 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,864 Location US GAL02 said: ... during PV Dwg.overlook. Click to expand... Isn't there a drawing of it, on the, uh, drawing? The problem with sloppy work is that the supply FAR EXCEEDS the demand Upvote 0 Downvote
GAL02 said: ... during PV Dwg.overlook. Click to expand... Isn't there a drawing of it, on the, uh, drawing? The problem with sloppy work is that the supply FAR EXCEEDS the demand
Mar 1, 2020 #6 hacksaw Mechanical Joined Dec 7, 2002 Messages 2,587 Location US How about a Slip-on Reducing Flange. Basically a standard WN flange shipped with a Reducing Flange for field fabrication, Upvote 0 Downvote
How about a Slip-on Reducing Flange. Basically a standard WN flange shipped with a Reducing Flange for field fabrication,
Mar 1, 2020 1 #7 HTURKAK Structural Joined Jul 22, 2017 Messages 3,371 'SRWN' flange stands for SELF REINFORCED WELDING NECK flange.. A nozzle with welding neck flange is assumed to be self-reinforced as long as additional reinforcement is not needed .. Upvote 0 Downvote
'SRWN' flange stands for SELF REINFORCED WELDING NECK flange.. A nozzle with welding neck flange is assumed to be self-reinforced as long as additional reinforcement is not needed ..