Paulista
Electrical
- Feb 7, 2005
- 83
I was contemplating building my own motor mounts, using a polyurethane(Shore 90)rod turned on a lathe to the right diameter bushing and embedding two SS threaded rods at either end.
Undersized holes would be drilled at either end of the polyurethane bushing, the appropriate glue introduced and then the threaded SS rods screwed down the same.
Will it work ? Which glue ?
Undersized holes would be drilled at either end of the polyurethane bushing, the appropriate glue introduced and then the threaded SS rods screwed down the same.
Will it work ? Which glue ?