I am modelling parison forming in the glass bottle manufacturing process. It is a transient problem with heat transfer between glass and blank mould. THe process involves very high temperatures (1200deg c) and very sudden cooling in 2 seconds.
The aim of the project is to get a better understanding of the blank temperatures.
Has anyone had experience in such a topic?