Can anyone recommend a good resource(s) for obtaining elastic and plastic geometry factors in regards to Linear Elastic Fracture Mechanics (LEFM) and Elastic Plastic Fracture Mechanics (EPFM) respectively?

thanks,
 
Replies continue below

Recommended for you

Rooke and Cartwright
Paris and Tada

haven't seen plastic geometry corrections ?

Quando Omni Flunkus Moritati
 
rb1957 has highlighted what are probably the best compendiums. Try also

Stress Intensity Factors Handbook
Murakami, 1987

Handbook of Stress Intensity Factors
Sih, 1973
 