Oct 10, 2003 #1 hot2000 Petroleum Joined Sep 13, 2003 Messages 12 Location TR Gents, What is the difference between A106 body to A352 LCC body valves? I know the working temperature of A352 is lower than A106 ... Is there something metallurgycal differences? thanks....
Gents, What is the difference between A106 body to A352 LCC body valves? I know the working temperature of A352 is lower than A106 ... Is there something metallurgycal differences? thanks....
Oct 17, 2003 #2 bmoorthy Mechanical Joined May 29, 2003 Messages 457 Location CA Are you sure about A 106. I think it has to be A 105.Normally the valve bodies are forged (such as A 105)or Cast (As in case of A216). Upvote 0 Downvote
Are you sure about A 106. I think it has to be A 105.Normally the valve bodies are forged (such as A 105)or Cast (As in case of A216).