hot2000

Petroleum
Sep 13, 2003
12
Gents,
What is the difference between A106 body to A352 LCC body valves?
I know the working temperature of A352 is lower than A106 ... Is there something metallurgycal differences?
thanks....

 
Replies continue below

Recommended for you

Are you sure about A 106. I think it has to be A 105.Normally the valve bodies are forged (such as A 105)or Cast (As in case of A216).
 