Hey, I have a sheet metal part on which I want to put a thread for a captive / non-losable bolt. The thread won't be load-bearing, but I need to know what is manufacturable. I have an M8 bolt and I want to use 2mm thick SS sheet metal. Is it doable? Is there a general rule for this when it comes to manufacturability?
 
Assuming you're wanting to use a standard M8 thread (1.25mm pitch), after threading and deburring you're likely to have less than one full thread remaining.

You'd be better off using a rivet-type stud, or a spot welded stud.
 
There are tap methods that don't use a drilled hole but just deform the metal making a bulge that is thicker for more threads. I believe that formdrill is one of them. This might give you enough local thickness for holding.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
It is commonly known that the minimum recommended thread engagement to make a strong connection for a component with a tapped hole is approximately 1 times the nominal diameter in steel and 2 times the nominal diameter in aluminum.

 