general practice of steelmaking of SA-105: fine grain practice? 4

Status
Not open for further replies.

YuJie_PV

Mechanical
Joined
Jan 19, 2017
Messages
152
Location
CN
hi all,
it is a question about steelmaking of SA-105.
i have an experience that the SA-105 I purchased are always normalized even without prior requirement.
and what about fine grain practice? will the Steel Mill perform fine grain practice as default?
In other words, what is general practice performed to SA-105 on fine grain practice?
anyone has any steelmaking experience in this?

Thanks in advance.
 
Never select SA-105 if you need fine grain.