My customer is asking to me the following:

GATE VALVE 150/RF BODY: A216 WCB AND TRIM UNS C 61300 WHERE CAN I FIND ANY VALVE WITH THOSE CHARACTERISTICS?

 
UNS C61300 is ASTM B169/B169M-05 - Aluminum Bronze.
 