Hi to All
The answer to the following question shall be greatly appreciated:
I am trying to install a SSDS (super Duplex)2500# RTJ flanged madular DB&B valve on a Flow Line using a 6"x 2"-2500# RTJ Nipoflange in A350 LF2 material (Flow line is API 5LX52N), now, What type of Gasket is the most appropriate between these two diffrent type of flanges ?, I am contemplating gaskets of type Octagonal Ring AISI 316 R26! will this be OK with regards to Corrosion?
Thanks a lot
 
Thanks Steve, no the line is not Subsea but it is on a platform at sea !
 
No, the Nipoflange is a standard 2500# RTJ and does not have any perticular weld overlay, if you mean the surface of the flange grooves has been treated. Do you mean the ring might corrode ?
Thanks.
 
Hi
I found out (in addition to your comments)that HARDNESS of the gasket in comparison with the 2 different type of surface material of the flanges, play a significant part when it comes to corrosion and leakage.
Thank you
 
Hi pipeneer, if your worried about corrosion, you can get specific gaskets that aid the joints resistance to corrosion.

Flexitallic make a flange rescue gasket in an RTJ form to fight corrosion.


Pikotech also make there VCS gaskets

There are a few others if you Google. Also due to the difference in metals across the flange ensure you get a full insulating kit for the whole joint (insulating bolt sleeves + washers), this will prevent galvanic corrosion.

Disclaimer:- I work for Flexitallic, but I am not a salesperson so am not promoting anything just trying to help.