Nov 18, 2005 #1 azzt Mechanical Joined May 19, 2004 Messages 32 Location GB Hi I am looking for information regarding the effects of liquid and sour gas fuel (compared to natural gas) on gas turbine blades cast in MAR-M-247. any help greatly appreciated Thanks allan
Hi I am looking for information regarding the effects of liquid and sour gas fuel (compared to natural gas) on gas turbine blades cast in MAR-M-247. any help greatly appreciated Thanks allan
Nov 28, 2005 #2 Goahead Aerospace Joined Jul 13, 2003 Messages 625 Location IL On cast Nickel base alloys it is customary to apply surface protective coatings against sulfidation (hot corrosion). See https://www.continuinged.purdue.edu/pdf/4218.pdfpara. 2.3.1.1 Regards, http://www.welding-advisers.com/ Upvote 0 Downvote
On cast Nickel base alloys it is customary to apply surface protective coatings against sulfidation (hot corrosion). See https://www.continuinged.purdue.edu/pdf/4218.pdfpara. 2.3.1.1 Regards, http://www.welding-advisers.com/