Is there any difference in corrosion protection for steel sheet hot-dip galvanized (zinc coated) vs. the heat-treated or "galvannealed" material that produces a zinc/Fe alloy at the surface? The environment is indoor and possibly outdoor on commercial buildings.

 
Replies continue below

Recommended for you

As long as they both have roughly equivalent thickness and zinc content, then there won't be much of a difference in the environments you describe.